Material Notes:
LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
1.21 g/cc
0.0437 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
0.0053 cm/cm

@Time 86400 sec
0.0053 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 117 MPa
17000 psi
ASTM D638
122 MPa
17700 psi
ISO 527
Tensile Strength, Yield 111 MPa
16100 psi
ISO 527
117 MPa
17000 psi
ASTM D638
Elongation at Break 2.1 %
2.1 %
ISO 527
2.2 %
2.2 %
ASTM D638
Elongation at Yield 2.1 %
2.1 %
ISO 527
2.2 %
2.2 %
ASTM D638
Tensile Modulus 8.96 GPa
1300 ksi
50 mm/min; ASTM D638
9.57 GPa
1390 ksi
1 mm/min; ISO 527
Flexural Strength 158 MPa
22900 psi
ASTM D790
184 MPa
26700 psi
ISO 178
Flexural Modulus 6.89 GPa
999 ksi
ASTM D790
7.75 GPa
1120 ksi
ISO 178
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.54 J/cm
16.0 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 52.0 kJ/m²
24.7 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 7.00 J
5.16 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 44.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 93.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 162 °C
324 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
161 °C

@Thickness 3.20 mm
322 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 158 °C
316 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
156 °C

@Thickness 3.20 mm
313 °F

@Thickness 0.126 in
unannealed; ASTM D648