Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin
(discontinued **) Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, MD | 8.30 MPa | 1200 psi | ASTM D882 |
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Film Tensile Strength at Yield, MD | 8.30 MPa | 1200 psi | ASTM D882 |
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |
|||
Film Tensile Strength at Yield, MD | 8.30 MPa | 1200 psi | ASTM D882 |
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi.. |
|||
Film Tensile Strength at Yield, MD | 8.30 MPa | 1200 psi | ASTM D882 |
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera.. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior prope.. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 302.32 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 302.34 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 302.56 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 312.09 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 312.23 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 312.82 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly.. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Availability: Latin America, North America and South America Addit.. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
Film Tensile Strength at Yield, MD | 8.27 - 13.0 MPa | 1200 - 1890 psi | Average value: 9.88 MPa Grade Count:24 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is .. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil Exceed™ 1015HA Metallocene Polyethylene Resin Product Description: Exceed 1015 mVLDPE resin is metallocene ethylene-hexene copolymer. Films made from Exceed 1015 mVLDPE have outstanding cold temperature toughness, impact strength and puncture. .. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, MD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil Exceed™ 4518CB Metallocene Polyethylene Resin Product Description: Exceed 4518 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 4518 have outstanding tensile properties and impact and puncture toughness. These superior p.. |
|||
Film Tensile Strength at Yield, MD | 8.30 MPa | 1200 psi | ASTM D882 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |