Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 345 MPa | 50000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated Steel FX-227-T Powdered Metal Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1005-50Information Provided by Pacific Sintered Metals, a division of PSM Ind.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-T Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-45Information Provided by Pacific Sintered Metals, a division.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | |
Materion BrushBronze® 95510 (AMS 4880) Centrifugal Cast 1.0" - 17.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 95510 is an Aluminum-Nickel-Bronze alloy that combines high strength, ductility, and good abrasion resistance under sever.. |
|||
Tensile Strength, Yield | 345 - 448 MPa | 50000 - 65000 psi | |
Meehanite Almanite® WS Wear and Abrasion Resisting Cast Iron Type WS is a hard wearing martensitic iron with exceptional impact strength...not readily machinable...work hardens in service to high hardness values. Type WS is recommended for crusher jaws, impa.. |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | |
MetalTek MTEK 175-B Cast UNS C95410 Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 %, Temperature 870 °C |
50000 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 214® alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 %, Temperature 870 °C |
50000 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | 0.2% proof |
Kobe Steel KSG12 Titanium alloy with low alloying elements, ASTM Gr. 12, Annealed Nominal Composition: Ti-0.3 Mo-0.8 Ni Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provid.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 %, Temperature 760 °C |
50000 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 %, Temperature 260 °C |
50000 psi @Strain 0.200 %, Temperature 500 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 345 - 427 MPa | 50000 - 62000 psi | 0.2% offset |
Eagle Brass 19210 XP-10 Copper Iron, 3/4 Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
Crucible Steel 430F Stainless Steel Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive environments. The chemistry is closely controlled to develop o.. |
|||
Tensile Strength, Yield | 345 - 517 MPa | 50000 - 75000 psi | |
Chicago Extruded Metals BioBrass® UNS C63000 Aluminum Bronze Finished product available as bar,rod, forged, shapes, or tubes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chica.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | |
CMW® DSC Copper with Dispersed Aluminum Oxide CMW® DSC material is an extruded and cold worked powder metallurgy material consisting of copper and dispersed aluminum oxide. It has exceptional high temperature strength for its electrical conduc.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | Annealed |
California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy All values may vary dependent on specific design and usage99.9% copper cladding over iron-nickel coreCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 345 - 372 MPa @Strain 0.200 %, Thickness 1.02 mm |
50000 - 54000 psi @Strain 0.200 %, Thickness 0.0402 in |
|
AK Steel 11 Cr-Cb™ Ferritic Stainless steel AK Steel 11 Cr-Cb™ has increased silicon levels and is dual stabilized with titanium and columbium. Designed for use in automotive exhaust tubing and other high-temperature applications, this is a.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.This is a soft ferritic material designed for operation in more corrosive environments than tolerated by 18% Cr-Fe Type 430 stainless. This new mat.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | Semi-Processed |
AK Steel DI-MAX® M-43 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | In rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | In rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | |
AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 1 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 345 - 517 MPa @Strain 0.200 % |
50000 - 75000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899A 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 345 - 517 MPa @Strain 0.200 % |
50000 - 75000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899M 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
Typical; Annealed Plate |
ATI Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022 AL 22 alloy is a Ni-Cr-Mo alloy that provides outstanding resistance to pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. The combination of Cr, Ni, Mo, and W provide.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allvac® Grade 12 UNS R53400 Titanium Alloy Uses: Industrial components. CPI equipment, heat exchangers, pressure vessels, fittings, tubing.Property values are for samples in the metallurgical condition: 1300°F anneal.Information provided by.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® C 22 UNS N06022 Nickel Superalloy Uses: Pressure vessels, pumps, valves, HX tubing and piping for the CPI and HPI. Trays, flanges, fasteners, wire, screens.Property values are for samples in the metallurgical condition: 2050°F age... |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | In rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | Beta Quenched |
ATI Wah Chang Tiadyne™ 3510 Capable of being surface hardened to depths that produce very high wear resistance. Produced by traditional metallurgical processing, not special treatments.Information provided by ATI Wah Chang |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 17-7™ High Strength Stainless Steel, UNS S17700 Property data below is typical of annealed samples. Available in sheet and strip. For use in high-strength springs, bellows, and aerospace applications.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |