Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.9 GPa | 2310 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne OnForce™ LFT UR-60 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 15.9 GPa | 2310 ksi | ASTM D638 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP), 30% Glass Fiber Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.The moldab.. |
|||
Tensile Modulus | 15.9 GPa | 2310 ksi | ASTM D 638 |
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Tensile Modulus | 15.9 GPa | 2310 ksi | ASTM D638 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Tensile Modulus | 15.9 GPa | 2310 ksi | dry; ISO 527 |
Ter Hell Plastic Terez® PA 6.6 7510 GF 50 Polyamide 66, 50% Glass Fiber Description: PA66 with medium viscosity, 50% glass fiber reinforced.Application: For molding parts with very high stiffness at good thermal stability.Information provided by Ter Hell Plastic GMBH... |
|||
Tensile Modulus | 15.9 GPa | 2310 ksi | ASTM D638 |
Plenco 6401 Phenolic, Briquette, Injection Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Tensile Modulus | 15.9 GPa | 2310 ksi | 1 mm/min |
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |
|||
Tensile Modulus | 15.9 GPa | 2310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 15.9 GPa | 2310 ksi | ASTM D638 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)
(Unverified Data**) Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili.. |
|||
Tensile Modulus | 15.9 GPa | 2310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 (Asia Pacific) LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Asia Pacific region. |