Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.60 GPa | 522 ksi | |
Plastcom SLOVALEN PH 78 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards detergents. General application in all industry branches.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | Type 1B, 50mm/min; ISO 527-1/2:1993 |
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled) This exceptional oil-loaded nylon features a complex blended oil lubrication system, uniformly distributed throughout the product, that guarantees constant performance over the whole service life. E.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 505RU PC Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East) Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex NS0039XP PC+ABS (Europe-Africa-Middle East) LNP* FARADEX* NS0039XP is a compound based on PC/ABS resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Electrically Conductive, EMI/RFI Shielding, Flame retardant.Thi.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East) CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527 |
Nilit FRIANYL A63 KG20 Nylon 6.6 for injection molding, 20% chalk filled Nylon 6.6 for injection molding (low warpage and good form stability).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | DIN 53457 |
Isoflon PEEK Polyetheretherketone Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® B 30 S F30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, flame retardantInformation provided by LANXESS. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RAL22 is a compound based on PA66 resin containing PTFE, Aramid Fiber. Added Features: Internally Lubricated |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527-1/-2 |
DSM Akulon® S223-D (Dry) Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/20 HWCP 10% Glass Fiber and 20% Glass Sphere Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/20 HWUVCP 10% Glass Fiber and 20% Glass Sphere Nylon 6, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000/505 GS 30 HWCP 30% Impact Modified Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336W40L1 Wollastonite Reinforced |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339G20M10CL Glass/Mineral Reinforced Coupled |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Cast Nylons Nycast® 6PA-MoS2 Nylon 6 NYCAST® 6PA-MoS2 is a molybdenum disulphide filled Type 6 cast nylon. Finely divided MoS2 particles are suspended in the melt during polymerization. This gives the NYCAST® 6PA-MoS2 products improv.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | |
BASF Procom® GC20S 400 Polypropylene Uses: electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 M Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |