Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 70.0 g | 0.154 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® H&T FHH 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex H&T FHH 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidant, suitable for blown film extrusion.Films obtained from Clearflex H&T FHH 508 show good op.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | F50; ISO 7765-1 |
Polimeri Europa Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion Eraclene FC 82 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully co.. |
|||
Dart Drop Test | >= 70.0 g | >= 0.154 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 70.0 g | 0.154 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-1117 LLDPE Film/Sandwich Bag Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin. Films made from LL-1117 have very good tensile properties and toughness. This resin's good strength and drawability all.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709 |
ExxonMobil LD 145.PX Packaging Resin
(discontinued **) LD 145.PX resin is a homopolymer cast film resin offering good clarity and toughness. Applications include Bread bags and other Food Packaging.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 70.0 g | 0.154 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-104 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer packaging film resin with excellent clarity and good stiffness. It is excellent either blown film or chill roll casting equipment. I.. |
|||
Dart Drop Test | 70.0 - 700 g | 0.154 - 1.54 lb | Average value: 270 g Grade Count:96 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-708 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15.5% vinyl acetate copolymer film resin. Film made from LD-708 exhibits good impact strength and superior heat sealability.Applications: Primal .. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709 |
Iran Petrochemical (PCC) 235F7 Linear Low Density Polyethylene 235F7 is a LLDPE blown film grade designed for general purpose film application. This resin is particularly suited for blending with LDPE, giving better strength and downgauging possibility.Informat.. |
|||
Dart Drop Test | 70.0 g @Thickness 0.0250 mm |
0.154 lb @Thickness 0.000984 in |
ISO 7765-1 |
Borealis FG5199 Linear Low Density Polyethylene FG5199 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-Fog and cling additives. The grade is developed for blown cling film. Film made from FG5199 is suit.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709 |
ExxonMobil LD 129.24 Cast Overwrap Film Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709A |
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709A |
ExxonMobil LDPE LD 129.24 Low Density Polyethylene Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709A |
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709A |
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1201KG Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1201XV Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | gF/50%f; ASTM D1709 |
Braskem EB853/72 Blown Film Extrusion Low Density Polyethylene Automatic packaging for several products; High transparency films.Additives: Antiblock, DInformation provided by Braskem. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | g/F50; ASTM D1709 |
Braskem F2022/0 Cast Film Extrusion Low Density Polyethylene Films for diapers and absorbent articles; Medium resistance films or for general use.Information provided by Braskem. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | ASTM-D1709 |
Braskem F2022/0 LDPE Cast Film Extrusion Polyethylene LDPE F2022/0 has excellent sealing characteristics and optical properties with well balanced mechanical properties. Its applications include: general purpose which require no additives; shrink film.. |
|||
Dart Drop Test | 70.0 - 290 g | 0.154 - 0.639 lb | Average value: 138 g Grade Count:14 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is .. |
|||
Dart Drop Test | 70.0 - 850 g | 0.154 - 1.87 lb | Average value: 226 g Grade Count:41 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |
|||
Dart Drop Test | 70.0 g | 0.154 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su.. |