Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LL 1002.32 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LL 1002x74 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LL 1002x79 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD >= 26.2 MPa
>= 3800 psi
ASTM D 882 A
Total Finathene® 6450 HDPE film  (discontinued **)
Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lin..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
LyondellBasell Petrothene® LP510300 High Density Polyethylene
ApplicationsPETROTHENE LLP 5103-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. It is r..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
Westlake Mxsten CV77529 Polyethylene Plastomer
Mxsten CV plastomer CV77529 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this ..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil Escorene® LD 713.93 Blown Film Resin
Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhibits very high impact strength, high clarity, and excellent heat sealability.Availability: Lat..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LL 1002.09 Blown Film Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LL 1002x75 Blown Film Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
Dow AFFINITY™ PL 1880 Polyolefin Plastomer
AFFINITY® PL 1880 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding packaging applications including high-speed, form-fill seal products. AFFINITY PL..