Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LL 1002.32 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LL 1002x74 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LL 1002x79 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | >= 26.2 MPa | >= 3800 psi | ASTM D 882 A |
Total Finathene® 6450 HDPE film
(discontinued **) Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lin.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
LyondellBasell Petrothene® LP510300 High Density Polyethylene ApplicationsPETROTHENE LLP 5103-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. It is r.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
Westlake Mxsten CV77529 Polyethylene Plastomer Mxsten CV plastomer CV77529 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this .. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil Escorene® LD 713.93 Blown Film Resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhibits very high impact strength, high clarity, and excellent heat sealability.Availability: Lat.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LL 1002.09 Blown Film Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LL 1002x75 Blown Film Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Break, TD | 26.2 MPa | 3800 psi | |
Dow AFFINITY™ PL 1880 Polyolefin Plastomer AFFINITY® PL 1880 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding packaging applications including high-speed, form-fill seal products. AFFINITY PL.. |