Flexural Yield Strength 42.0 - 260 MPa

@Temperature -40.0 - 150 °C
6090 - 37700 psi

@Temperature -40.0 - 302 °F
Average value: 109 MPa Grade Count:2
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Flexural Yield Strength 42.0 - 260 MPa

@Thickness 0.800 - 3.17 mm
6090 - 37700 psi

@Thickness 0.0315 - 0.125 in
Average value: 109 MPa Grade Count:2
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Flexural Yield Strength 68.9 - 260 MPa
10000 - 37700 psi
Average value: 139 MPa Grade Count:37
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Flexural Yield Strength 240 - 260 MPa

@Temperature 80.0 - 80.0 °C
34800 - 37700 psi

@Temperature 176 - 176 °F
Average value: 253 MPa Grade Count:4
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Flexural Yield Strength 11.5 - 260 MPa
1670 - 37700 psi
Average value: 172 MPa Grade Count:193
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Flexural Yield Strength 90.0 - 260 MPa
13100 - 37700 psi
Average value: 176 MPa Grade Count:91
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Flexural Yield Strength 110 - 260 MPa
16000 - 37700 psi
Average value: 177 MPa Grade Count:43
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..