Mechanical Properties Metric English Comments
Compressive Strength 25.0 - 35.0 MPa

@Temperature 100 °C
3630 - 5080 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1000 °C
3630 - 5080 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 100 °C
3630 - 5080 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 110 Dense Refractory Castable
Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 100 °C
3630 - 5080 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1000 °C
3630 - 5080 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 HS Dense Refractory Castable
Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars...
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1200 °C
3630 - 5080 psi

@Temperature 2190 °F
Cold Crushing Strength
Gouda Vuurvast CURON 130 Dense Refractory Castable
Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 100 °C
3630 - 5080 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 140 GM Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1300 °C
3630 - 5080 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 140 GM Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1300 °C
3630 - 5080 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 HS GM Dense Refractory Castable
Description: Curon 150 HS GM is an abrasion resistant gunning castable for use up to 1500°C.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1300 °C
3630 - 5080 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable
Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1600 °C
3630 - 5080 psi

@Temperature 2910 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 T SP GM Dense Refractory Castable
Description: Curon 180 T SP GM is a gunning castable based on tabular alumina for application at very high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuu..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 100 °C
3630 - 5080 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 100 Dense Refractory Castable
Description: Curon 100 is a general purpose castable for temperatures up to 1000°C.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modification..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1300 °C
3630 - 5080 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 H Dense Refractory Castable
Description: Curon 150 H is composed of a very pure grog combined with a high quality high alumina cement. It is characterized by a good resistance against thermal shock and against reducing operati..
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1300 °C
3630 - 5080 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 165 Dense Refractory Castable
Description: Curon 165 is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Also availa..