Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 25.0 MPa @Strain 3.30 %, Temperature 100 °C |
3630 psi @Strain 3.30 %, Temperature 212 °F |
Y direction, Condition A; ASTM D695 |
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Compressive Strength | 25.0 MPa @Strain 1 % |
3630 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data) Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit.. |
|||
Compressive Strength | 25.0 MPa @Strain 5 % |
3630 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Compressive Strength | 25.0 MPa @Strain 2 % |
3630 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Semitron® ESd 225 POM-C, static dissipative, extruded (ISO Data) Semitron ESd 225 is an acetal based static dissipative material ideal for material handling operations. It is also an excellent choice for fixturing used in the manufacturing of hard disk drives or .. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 100 °C |
3630 - 5080 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 1000 °C |
3630 - 5080 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 100 °C |
3630 - 5080 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 110 Dense Refractory Castable Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 100 °C |
3630 - 5080 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 120 Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 1000 °C |
3630 - 5080 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 120 HS Dense Refractory Castable Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars... |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 1200 °C |
3630 - 5080 psi @Temperature 2190 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 130 Dense Refractory Castable Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 100 °C |
3630 - 5080 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 140 GM Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 1300 °C |
3630 - 5080 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 140 GM Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 1300 °C |
3630 - 5080 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 HS GM Dense Refractory Castable Description: Curon 150 HS GM is an abrasion resistant gunning castable for use up to 1500°C.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 1300 °C |
3630 - 5080 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 1600 °C |
3630 - 5080 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 T SP GM Dense Refractory Castable Description: Curon 180 T SP GM is a gunning castable based on tabular alumina for application at very high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuu.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 100 °C |
3630 - 5080 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 100 Dense Refractory Castable Description: Curon 100 is a general purpose castable for temperatures up to 1000°C.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modification.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 1300 °C |
3630 - 5080 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 H Dense Refractory Castable Description: Curon 150 H is composed of a very pure grog combined with a high quality high alumina cement. It is characterized by a good resistance against thermal shock and against reducing operati.. |
|||
Compressive Strength | 25.0 - 35.0 MPa @Temperature 1300 °C |
3630 - 5080 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 165 Dense Refractory Castable Description: Curon 165 is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Also availa.. |
|||
Compressive Strength | 25.0 MPa @Strain 1 % |
3630 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data) Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte.. |