Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled 30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector |
|||
Flexural Modulus | 8.24 GPa | 1190 ksi | 5 mm/min; ISO 178 |
Gromax BFG30-AH00B2 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK (Europe-Africa-Middle East) LNP*LUBRICOMP* LFL36 is a compound based on Polyetheretherketone resin containing Glass Fiber, PTFE.
Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
Solvay TECHNYL® A 718 V30 PA66, 30% glass fiber, DRY Description: TECHNYL A 718 V30 is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moldingColors: it is sailed on natural and black colorAvailable in: Latin AmericaMai.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36S PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON WC003 PBT (Europe-Africa-Middle East) LNP* Stat-kon* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 8.24 GPa | 1190 ksi | |
Shinil Chemical SHINFLAME PBT GF Flame Retardant Polymer Lamp Housing SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Asia Pacific) Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF0067K PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF0067K is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | |
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Flexural Modulus | 8.19 GPa | 1190 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Unitika AXG-1500-300 Dry Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Plenco 4485 Phenolic, Granular, Compression Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM-D790 |
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GVZ 30 HWCP 30% Glass Fiber Z-Qualities Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Zytel 77G33L BK031 is a 33% glass fiber reinforced black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide PF006ES PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF006ES is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO Value |
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he.. |
|||
Flexural Modulus | 8.20 GPa @Temperature 60.0 °C |
1190 ksi @Temperature 140 °F |
ASTM D790 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
PlastxWorld CEVIAN® B2506 30% GF PBT/ABS Alloy Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Plenco 6527 Phenolic, Granular, Injection Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Flexural Modulus | 8.21 GPa | 1190 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON PX00700 PA 6 LNP VERTON* PX00700 is a compound based on Nylon 6 resin containing proprietary fillers. Added feature of this grade is: Structural. |