Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer
Manufacturer Proto3000
Trade Name Objet Digital Materials™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the desired mechanical properties and to resemble the product’s target materials.Information provided by Proto3000 for their protoyping engineering services.
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 - 65.0 MPa
7250 - 9430 psi
ASTM D638-03
Elongation at Break 10 - 25 %
10 - 25 %
ASTM D638-05
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Flexural Strength 75.0 - 110 MPa
10900 - 16000 psi
ASTM D790-03
Flexural Modulus 2.20 - 3.20 GPa
319 - 464 ksi
ASTM D790-04
Izod Impact, Notched 0.200 - 0.300 J/cm
0.375 - 0.562 ft-lb/in
ASTM D256-06
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 - 50.0 °C
113 - 122 °F
ASTM D648-06