Material Notes:
FD60-018 is a very high molecular weight high density polyethylene powder. It exhibits very high impact strength.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D4883
Apparent Bulk Density 0.480 g/cc
0.0173 lb/in³
ASTM D1895
Melt Flow 1.7 g/10 min
1.7 g/10 min
190 / 21.6 (HLMI); ASTM D1238
<= 0.10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
<= 0.10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Break 910 %
910 %
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 131 °C
268 °F
ASTM D1525
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746