Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 105 °C | 221 °F | TM R050-25 |
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | 10°C/min test |
Polimeri Europa SINKRAL G320 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 General purpose injection moulding grade with good impact resistance, good flow and high gloss. SI.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | 10°C/min test |
Polimeri Europa SINKRAL PD M323 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose injection moulding grade that exhibits outstanding flow and thermal stability duri.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Eastman Tenite 383A-10 Cellulose Acetate Propionate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Mallard Creek Polymers Rovene® 6115 Resin Supported Emulsion Rovene® 6115 is a hard, non-film forming vehicle that is neutralized with sodium hydroxide for flexographic and gravure inks and overprint varnishes primarily for use on paper and paperboard subs.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | ASTM D3418 |
Kolon DIAMAT® IG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | Perkin-Elmer DSC-2 |
Lord Adhesives Thermosetâ„¢ MD-200 Electrically Conductive Die-Attach Adhesive This is a system with the versatility to fit a wide variety of production and performance needs. The working life allows sufficient time for short production interruption. It can be initially cured .. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | MCI Method |
Mitsui APELâ„¢ APL6011T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Lucite International Colacryl ® LS200 Specialty Acrylic Resin Colacryl® LS200 is a medium-high molecular weight methyl methacrylate polymer. It is used mainly in coating applications where abrasion resistance and resistance to plasticiser migration are impo.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Lucite International Colacryl ® TS2082 Acrylic Resin Colacryl® TS2082 is a solid bead resin with low residual peroxide content, specially designed for use in a variety of industrial and dental applications. In dental applications the product is typ.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Lucite International Elvacite ® 2008 Acrylic Resin Elvacite® 2008 is a low molecular weight methyl methacrylate copolymer. It is used in lacquers and gravure inks requiring low viscosity at high solids. 2008 provides good activity for pigment dis.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Lucite International Elvacite ® 2051 Acrylic Resin Elvacite® 2051 is a high molecular weight methyl methacrylate polymer. It is used in many coatings applications providing maximum abrasion resistance, block resistance, and slip. It is non-reacti.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Lucite International Elvacite ® 3000 Acrylic Resin Elvacite® 3000 is a solid bead resin specially designed for use in coatings and inks on a variety of substrates. It has fair compatibility with many binders and plasticisers, and has excellent so.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | wet |
Henkel Hysol PL 696 Film Adhesive Epoxy-based structural film adhesive designed primarily for out-of-autoclave curing process applications requiring low cure temperatures as well as low curing pressures and is also available in ligh.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Lucite International Elvacite ® 2041 Acrylic Resin Elvacite® 2041 is a high molecular weight methyl methacrylate polymer. It is used in many coatings applications providing maximum abrasion resistance, block resistance, and slip. It is non-reacti.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Styron DL 247A Plastic Pigment Performance Features: Oil well, gas blocking, high temperature gas migration controlApplications: Modified ConcreteNorth AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Styron DL 247NA Carboxylated SB Performance Features: Firm hand additiveApplications: Thermo MoldableLatin America/South AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | |
Zeon Chemicals Zeonor® 1020R Cyclo-Olefin Polymer Zeonor 1060R shall be in the form of pellets. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | Ultimate Tg; TMA |
Tra-Con Supertherm 826M01 High Performance Diamond Epoxy Adhesive SUPERTHERM 826M01 is a one-part, smooth paste ULTRA HIGH THERMALLY CONDUCTIVE diamond filled epoxy adhesive recommended for semiconductor die-attach and other micro-electronic applications where the.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | Ultimate Tg |
Tra-Con Tra-Bond F118 Fiber Optic Epoxy Adhesive TRA-BOND F118 is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows mor.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | Ultimate Tg |
Tra-Con Tra-Bond F118CLR Fiber Optic Epoxy Adhesive TRA-BOND F118CLR is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows .. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | Ultimate Tg |
Tra-Con Tra-Duct 921M01 Low Viscosity Long Pot Life Silver-Filled Epoxy TRA-DUCT 921M01 is a two component, silver-filled electrically conductive epoxy adhesive designed for applications which require electrical conductivity and a long pot life at a relatively low heat .. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | dynamic; DIN 53 736 |
Hippe PMMA Components made of PMMA are brilliantly transparent. Outstanding aging stability and weathering resistance. Good surface hardness. Abrasion-resistant. Physiologically safe. High strength. Easi.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | 10°C/min test |
Polimeri Europa SINKRAL D720 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-08-35-15 High impact injection moulding grade, with improved flow compared with SINKRAL B620 and a high glo.. |
|||
Glass Transition Temp, Tg | 105 °C | 221 °F | 10°C/min test |
Polimeri Europa SINKRAL L320/G ABS, Platable Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-20 Injection moulding grade, tailored for electroplating. It is a high flow grade with a good impact .. |
|||
Glass Transition Temp, Tg | 105 - 110 °C | 221 - 230 °F | Average value: 107 °C Grade Count:3 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |