Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Asia Pacific) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications.This data was supplied by SABIC-IP for th.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C6200 is a non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. C6200 has improved processing window and edge crac.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 6.60 mm |
167 °F @Thickness 0.260 in |
UL 746 |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | |
PTS 15GFR-BK PBT- Flame Retardant, 15% Glass Filled PBT Black Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | |
PTS PCA-3013 High Flow PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | |
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical with Impact | 75.0 - 130 °C | 167 - 266 °F | Average value: 112 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
UL RTI, Mechanical with Impact | 75.0 - 140 °C | 167 - 284 °F | Average value: 113 °C Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | |
PTS 30GFR-BK PBT- Flame Retardant, 30% Glass Filled PBT Black Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical with Impact | 75.0 - 115 °C | 167 - 239 °F | Average value: 111 °C Grade Count:11 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
UL RTI, Mechanical with Impact | 75.0 - 130 °C | 167 - 266 °F | Average value: 107 °C Grade Count:9 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | |
Covestro Bayblend® FR 2000 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746B |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Europe-Africa-Middle East) NORYL SE90 is an unfilled, flame retardant material with a Vicat B/120 of 110°C according ISO 306. NORYL SE90 is V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Valox® 364 PBT+PC Designed for outdoor telecommunications enclosure applications. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
|
Covestro Bayblend® FR 90 N Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sepa.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
|
Covestro Bayblend® FR 90 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | UL 746B |
Covestro Makroblend® UT305 PC/PET Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• High moisture en.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C | 167 °F | |
Covestro Makrolon® 8325 Polycarbonate High viscosity injection molding and extrusion grade with 20% standard glass fibers and easy mold release, high strength and stiffness.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Rynite® 515CS BK575M PET Rynite® 515CS BK575M is a 15% glass fiber reinforced, black polyethylene terephthalate resin modified for improved color stability after heat aging.Information provided by DuPont Performance Polyme.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
UL 746B |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.57 mm |
167 °F @Thickness 0.0618 in |
|
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant