Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Tenite Polyethylene 1810A Low Density Polyethylene - Molding  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Tenite Polyethylene 1810A Low Density Polyethylene - Molding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: TENITE Polyethylene 1810A contains NO ADDITIVES. It is suggested for injection molding applications. TENITE Polyethylene 1810A meets the requirements of FDA regulation 21 CFR 177.1520(c)(2.2) and may be used as a component of packages used for holding food during cooking.Technical Data Sheet Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.Information provided by Eastman Chemical.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D4883
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.8 MPa
2000 psi
500 mm/min (20 in./min); ASTM D638
Tensile Strength, Yield 11.0 MPa
1600 psi
500 mm/min (20 in./min); ASTM D638
Elongation at Break 500 %
500 %
500 mm/min (20 in./min); ASTM D638
Flexural Modulus 0.221 GPa
32.1 ksi
2% Secant; ASTM D 790
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Brittleness Temperature -73.0 °C
-99.4 °F
ASTM D746