Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | ASTM D648 |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | |
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C @Thickness 6.40 mm |
563 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C @Thickness 6.40 mm |
563 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | Unannealed; Flatwise; ISO 75-2/A |
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | ASTM D648 |
DuPont Performance Polymers VESPEL TP-8161 Polyimide DuPont Vespel TP-8161 parts are specified for high-temperature applications. TP-8161 parts offer a unique balance of mechanical and thermal properties for superior performance in aggressive environm.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | |
LATI Latilub 88/50-20GRT K/10 PEEK, 10% Carbon Fiber Reinforced, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | ASTM D648 |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | ASTM D648 |
E-Polymers SEPAZ® C245GP 45% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 295 °C | 563 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry
(discontinued **) Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |