Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber Natural color. E6666 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati.. |
|||
Front Barrel Temperature | 260 - 302 °C | 500 - 575 °F | |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
PTS Tristar® PC-10R-(18) 18 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 260 - 302 °C | 500 - 575 °F | |
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
Ravago Manufacturing Americas Hybrid S470H Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Flame Retardant RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)
(discontinued **) Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa PA6-MG30 30% Glass & Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 260 - 275 °C | 500 - 527 °F | |
Lavergne VYTEEN PC/ABS 3016 PC-ABS, 16% Glass Reinforced Vyteen PC/ABS 3016 is a black 16% glass fiber reinforced Polycarbonate/ABS alloy designed for injection molding.Features: -Good processability -Balanced stiffness/resilience -High deflection temp.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa CPA-6 Toughened PA6 Features:High impactLow tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® B 230 PA66/6, DRY Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1002 Polyarylamide (PARA), 30% Glass Fiber Ixef® 1002 is a 30% glass-fiber reinforced, general purpose polyarylamide compound which exhibits high strength and rigidity, outstanding surface finish, and excellent creep resistance.Features: .. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Teknor Apex Beetle® PET166F Polyethylene Terephthalate, 30% Glass Fiber Reinforced Notes: PET166F is a 30% glass fiber reinforced grade of PET that offers good mechanical performance at elevated temperature and excellent mold release. Processing Method: Injection Molding Forms: Pe.. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 Impact Modified Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 277 °C | 500 - 530 °F | |
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Front Barrel Temperature | 260 - 277 °C | 500 - 530 °F | |
Wellman Wellamid® GSF25/15-66 22L-N 40% Glass Sphere/Fiber Reinforced Nylon 66 Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, at Equilibrium (65% RH)
(discontinu The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
Beijing Chemical Industry KAIFA® MN101 Nylon 66 Resin Good flow, High impactInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |