Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Front Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Start Point: 250°C |
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Start Point: 245°C |
Kingfa LONOY 1200 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Start Point: 260°C |
Kingfa LONOY 1600 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Start Point: 260°C |
Kingfa LONOY 6100 Flame Retardant PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant Feature: Injection Molding, PA6+GF15%, Flame RetardantApplication: ConnectorsCAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Front Barrel Temperature | 235 - 270 °C | 455 - 518 °F | Injection Molding |
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
Lavergne VYTEEN PC/ABS 8515 Polycarbonate - Acrylonitrile Butadiene Styrene Alloy Vyteen PC/ABS 8515 is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High def.. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
Lavergne VYTEEN PC/ABS 8515XF Polycarbonate - Acrylonitrile Butadiene Styrene Alloy Vyteen PC/ABS 8515XF is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High d.. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Start Point: 260°C |
Kingfa LONOY 2100 LT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® B 238 Black 21 N PA66/6, DRY Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular.. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Pre-3. Region Temperature |
Tisan TISARBON® Flame Retardant (V0) Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Pre-3. Region Temperature |
Tisan TISARBON® UNR Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Zone 3 |
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Zone 3 |
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Zone 3 |
Eurostar Starflam PF0047E PA6, 20% Glass Filled, Injection Molded Starflam PF0047E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as EXCP4009)Information provided by Polymer Tech.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Zone 3 |
Eurostar Starflam PK0022E PA6, 10% Mineral Filled, Injection Molded PK0022E is a Halogen Free and Phosphorous Free, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3620Z22 or PA 10E6 U9 Z22)Information provided by Polymer Technology & Services, the Nor.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Zone 3 |
Eurostar Starflam PK0052E PA6, 25% Mineral Filled, Injection Molded PK0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3520Z222 or PA 25E6 U9 Z22)Information provided by Polymer Technolo.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Zone 3 |
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
Front Barrel Temperature | 265 - 270 °C | 509 - 518 °F | |
Beijing Chemical Industry KAIFA® MN301-G20 Nylon 66 Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Front Barrel Temperature | 265 - 270 °C | 509 - 518 °F | |
Beijing Chemical Industry KAIFA® MN301-G25 Nylon 66 Resin 25% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Front Barrel Temperature | 265 - 270 °C | 509 - 518 °F | |
Beijing Chemical Industry KAIFA® MN301-G35 Nylon 66 Resin 35% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |