Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 45.0 °C | 113 °F | optimum; Injection Molding |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Mold Temperature | 45.0 - 55.0 °C | 113 - 131 °F | Injection Molding |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Mold Temperature | 45.0 °C | 113 °F | optimum; Injection Molding |
DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET
(Unverified Data**) Hytrel® 6646 NC010 is a medium modulus grade with nominal hardness of 66D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like .. |
|||
Mold Temperature | 45.0 °C | 113 °F | Optimum; Injection Molding |
DuPont Performance Polymers Hytrel® 5553FG NC010 TPC-ET
(Unverified Data**) Hytrel® 5553FG NC010 is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont |
|||
Mold Temperature | 45.0 - 55.0 °C | 113 - 131 °F | Injection Molding |
DuPont Performance Polymers Hytrel® 5553FG NC010 TPC-ET
(Unverified Data**) Hytrel® 5553FG NC010 is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont |
|||
Mold Temperature | 45.0 °C | 113 °F | optimum; Injection Molding |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET
(Unverified Data**) Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In.. |
|||
Mold Temperature | 45.0 - 55.0 °C | 113 - 131 °F | Injection Molding |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET
(Unverified Data**) Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In.. |
|||
Mold Temperature | 45.0 °C | 113 °F | Optimum; Injection Molding |
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET
(Unverified Data**) Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont |
|||
Mold Temperature | 45.0 °C | 113 °F | optimum; Injection Molding |
DuPont Performance Polymers Hytrel® HTR8223 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8223 BK320 is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 42D, is pigmented black with fine particle size carbon black, a.. |
|||
Mold Temperature | 45.0 °C | 113 °F | optimum; Injection Molding |
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET
(Unverified Data**) Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,.. |
|||
Mold Temperature | 45.0 - 60.0 °C | 113 - 140 °F | |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Mold Temperature | 45.0 °C | 113 °F | |
Lubrizol Advanced Materials Pearlthane® Clear 15N60D Thermoplastic Polyurethane
(discontinued **) Polyester-based TPU, supplied in form of translucent, colorless or slightly yellowish pellets, combining very high hardness with excellent mechanical properties and excellent hyrdrolysis resistance... |
|||
Mold Temperature | 45.0 - 65.0 °C | 113 - 149 °F | Injection Molding |
Ineos ABS Lustran® 266 ABS, Transparent Grade Lustran® ABS 266 resin is a clear injection molding grade of ABS (acrylonitrile butadiene styrene). This transparent, general-purpose grade provides clarity and toughness with ease of processing... |
|||
Mold Temperature | 45.0 - 65.0 °C | 113 - 149 °F | Injection Molding |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Mold Temperature | 45.0 - 65.0 °C | 113 - 149 °F | Injection Molding |
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi.. |
|||
Mold Temperature | 45.0 - 80.0 °C | 113 - 176 °F | Injection Molding |
LG Chemical LUPOY RF3208F PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2 and 13463-67-1Information provided by LG .. |
|||
Mold Temperature | 45.0 - 60.0 °C | 113 - 140 °F | |
LATI Latiohm 82-02 PD09 PA12 Semiconductive/dissipative product based on Polyamide 12 (PA12). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Mold Temperature | 45.0 - 60.0 °C | 113 - 140 °F | |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Mold Temperature | 45.0 °C | 113 °F | ISO 294 |
Styrolution PS 485N HIPS Styrolution PS 485N is a high impact grade of polystyrene for extruded sheets with a matte surface.Matte SurfaceUL 94 HBInformation provided by Styrolution |
|||
Mold Temperature | 45.0 - 100 °C | 113 - 212 °F | |
Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66 Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Mold Temperature | 45.0 °C | 113 °F | optimum; Injection Molding |
DuPont Performance Polymers Hytrel® DYM1300 BK320 TPC-ET
(Unverified Data**) Hytrel® DYM1300 is a high performance thermoplastic elastomer with high modulus, suited for air bag door applications.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 45.0 °C | 113 °F | optimum; Injection Molding |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Mold Temperature | 45.0 - 55.0 °C | 113 - 131 °F | Injection Molding |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Mold Temperature | 45.0 °C | 113 °F | optimum; Injection Molding |
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET
(Unverified Data**) Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon.. |
|||
Mold Temperature | 45.0 °C | 113 °F | optimum; Injection Molding |
DuPont Performance Polymers Hytrel® HTR8241 TPC-ET
(Unverified Data**) Hytrel® HTR8241 is a 65 nom.Shore D, non discoloring stabilizer, plasticiser free high performance resin for extrusion; high viscosity; outstanding mechanical properties up to 120°C and excellent .. |
|||
Mold Temperature | 45.0 - 55.0 °C | 113 - 131 °F | Injection Molding |
DuPont Performance Polymers Hytrel® HTR8241 TPC-ET
(Unverified Data**) Hytrel® HTR8241 is a 65 nom.Shore D, non discoloring stabilizer, plasticiser free high performance resin for extrusion; high viscosity; outstanding mechanical properties up to 120°C and excellent .. |
|||
Mold Temperature | 45.0 °C | 113 °F | optimum; Injection Molding |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |
|||
Mold Temperature | 45.0 - 55.0 °C | 113 - 131 °F | Injection Molding |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |
|||
Mold Temperature | 45.0 °C | 113 °F | Optimum; Injection Molding |
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET
(Unverified Data**) Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont |
|||
Mold Temperature | 45.0 - 55.0 °C | 113 - 131 °F | Injection Molding |
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET
(Unverified Data**) Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont |