Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan.. |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym.. |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a P.. |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)
(Unverified Data**) Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also.. |
|||
Melt Temperature | 325 - 350 °C | 617 - 662 °F | |
Covestro Apec® DP9-9371 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Melt Temperature | 325 - 350 °C | 617 - 662 °F | |
Covestro Apec® DP9-9373 High-Heat Polycarbonate, General Purpose, UV-Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA) Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also.. |
|||
Melt Temperature | 325 - 340 °C | 617 - 644 °F | |
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melt Temperature | 325 - 340 °C | 617 - 644 °F | |
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melt Temperature | 325 - 340 °C | 617 - 644 °F | |
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melt Temperature | 325 - 340 °C | 617 - 644 °F | |
Akro-Plastic Akromid® T6 GF30 (3501) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melt Temperature | 325 - 340 °C | 617 - 644 °F | |
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melt Temperature | 325 - 340 °C | 617 - 644 °F | |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA) Zytel® HTN54G35EF NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin, developed for electrical and electronics applications. It is also a PPA r.. |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |
|||
Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE8200 BK431 is an unreinforced, toughened, heat stabilized, lubricated high performance polyamide resin for injection molding. It is also a PPA resin.Information provided by DuPont Perfo.. |