Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, a viscosity of 300 cps., and a weight of 7.8 lbs/gallon. AboCast 7802-1/AboCure 50-3 has versatility, many variable-ratio possibilities, and a tenacious adhesion to metals, ceramics, glass, wood, and most rigid materials which permits permanent structural and dielectric bonds. Absence of volatiles and minimum shrinkage, typical of solventless epoxy systems, allow castings and masses of virtually any desired thickness. Suggested Uses: Multi-purpose casting, coating, and bonding for applications requiring high dielectric resistance, structural strength, and radiation resistance as well as resistance to weather, water, alkalis, diluted acids, fuels, and most common solvents; it was originally developed for FERMILAB.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
AboCure 50-3
1.09 g/cc
0.0394 lb/in³
AboCast 7802-1
Water Absorption 0.10 - 0.30 %
0.10 - 0.30 %
Viscosity 500 - 700 cP
500 - 700 cP
blended
Mechanical Properties Metric English Comments
Hardness, Shore D 75

@Temperature 100 °C,
Time 10800 sec
75

@Temperature 212 °F,
Time 3.00 hour
75

@Temperature 100 °C,
Time 10800 sec
75

@Temperature 212 °F,
Time 3.00 hour
1/8 in thickness
<= 10

@Time 86400 sec
<= 10

@Time 24.0 hour
1/8 in thickness
20

@Time 259000 sec
20

@Time 72.0 hour
1/8 in thickness
20

@Time 86400 sec
20

@Time 24.0 hour
65

@Time 259000 sec
65

@Time 72.0 hour
Tensile Strength at Break 34.5 - 48.3 MPa
5000 - 7000 psi
Elongation at Break 10 - 15 %
10 - 15 %
Flexural Strength 62.1 - 82.7 MPa
9000 - 12000 psi
Compressive Strength 48.3 - 55.2 MPa
7000 - 8000 psi
Electrical Properties Metric English Comments
Dielectric Strength 15.7 - 19.7 kV/mm
400 - 500 kV/in
Processing Properties Metric English Comments
Pot Life 300 min
300 min
100 g
Descriptive Properties Value Comments
Parts by Weight (pbw) 100
AboCast 7802-1
40
AboCure 50-13
Users viewing this material also viewed the following: