Electrical Properties Metric English Comments
Dielectric Strength 19.7 - 24.0 kV/mm
500 - 610 kV/in
Average value: 21.1 kV/mm Grade Count:3
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Dielectric Strength 19.7 - 24.0 kV/mm
500 - 610 kV/in
Average value: 22.3 kV/mm Grade Count:5
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Dielectric Strength 17.7 - 24.0 kV/mm
450 - 610 kV/in
Average value: 21.0 kV/mm Grade Count:4
Overview of materials for Polyamide-Imide, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp..
Dielectric Strength 13.8 - 24.0 kV/mm
350 - 610 kV/in
Average value: 16.0 kV/mm Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Dielectric Strength 16.9 - 24.0 kV/mm
430 - 610 kV/in
Average value: 21.2 kV/mm Grade Count:4
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Dielectric Strength 7.44 - 24.0 kV/mm
189 - 610 kV/in
ASTM D149
Zeus PTFE Tubing
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,..
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON M-300H PCTFE Granular Molding Powder
NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Granular powders.Processing Methods: Compression molding, extrusion.Uses: Sheets, rods, tubing.Information provided by..
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON M-300P PCTFE Pellets
NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Pellets.Processing Methods: Extrusion.Uses: Rods, small parts.Information provided by Daikin Industries.
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON M-400H PCTFE Granular Molding Powder
NEOFLON PCTFE M-400 series is a high molecular weight type material which is suitable for applications requiring mechanical toughness and stress crack resistance.Description:Granular powders.Process..
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON NP-101 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro..
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON NP-120 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes..
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON NP-130 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka..
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON NP-21 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion ..
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON NP-30 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing..
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON NP-40 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s..
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON NP-20 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,..
Dielectric Strength 20.0 - 24.0 kV/mm

@Thickness 3.20 mm
508 - 610 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin NEOFLON NP-3000 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi..
Dielectric Strength 19.7 - 24.0 kV/mm
500 - 610 kV/in
Average value: 21.4 kV/mm Grade Count:7
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Dielectric Strength 12.0 - 24.0 kV/mm

@Temperature 95.0 - 200 °C
305 - 610 kV/in

@Temperature 203 - 392 °F
Average value: 18.9 kV/mm Grade Count:2
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Dielectric Strength 12.0 - 24.0 kV/mm

@Thickness 1.57 - 3.20 mm
305 - 610 kV/in

@Thickness 0.0618 - 0.126 in
Average value: 18.9 kV/mm Grade Count:2
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Dielectric Strength 18.0 - 24.0 kV/mm
457 - 610 kV/in
Average value: 22.5 kV/mm Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..