Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group 2567 AMC Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and .. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very .. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group RALUPOL® 4806 UP Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Dielectric Strength | 16.1 - 35.0 kV/mm | 409 - 889 kV/in | Average value: 25.6 kV/mm Grade Count:6 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Dielectric Strength | 17.7 - 35.0 kV/mm | 450 - 889 kV/in | Average value: 23.9 kV/mm Grade Count:12 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Dielectric Strength | 17.7 - 35.0 kV/mm | 450 - 889 kV/in | Average value: 23.6 kV/mm Grade Count:11 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Dielectric Strength | 15.7 - 35.0 kV/mm | 400 - 889 kV/in | Average value: 21.3 kV/mm Grade Count:25 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Dielectric Strength | 15.0 - 35.0 kV/mm | 380 - 889 kV/in | Average value: 28.4 kV/mm Grade Count:20 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Dielectric Strength | 16.0 - 35.0 kV/mm | 406 - 889 kV/in | Average value: 29.1 kV/mm Grade Count:29 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Dielectric Strength | 14.9 - 35.0 kV/mm | 378 - 889 kV/in | Average value: 24.6 kV/mm Grade Count:69 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Dielectric Strength | 14.0 - 35.0 kV/mm | 356 - 889 kV/in | Average value: 22.1 kV/mm Grade Count:49 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Dielectric Strength | 8.60 - 35.0 kV/mm | 218 - 889 kV/in | Average value: 17.7 kV/mm Grade Count:20 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Dielectric Strength | 19.7 - 35.0 kV/mm | 500 - 889 kV/in | Average value: 24.6 kV/mm Grade Count:18 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Dielectric Strength | 19.0 - 35.0 kV/mm | 483 - 889 kV/in | Average value: 26.6 kV/mm Grade Count:12 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | Average value: 29.2 kV/mm Grade Count:6 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Dielectric Strength | 21.0 - 35.0 kV/mm | 533 - 889 kV/in | Average value: 27.5 kV/mm Grade Count:4 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Dielectric Strength | 30.0 - 35.0 kV/mm | 762 - 889 kV/in | Average value: 32.0 kV/mm Grade Count:12 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Dielectric Strength | 6.00 - 35.0 kV/mm | 152 - 889 kV/in | Average value: 20.3 kV/mm Grade Count:3 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Dielectric Strength | 30.0 - 35.0 kV/mm | 762 - 889 kV/in | DIN 53481 |
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | 17.7 - 35.0 kV/mm | 450 - 889 kV/in | Average value: 23.9 kV/mm Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Dielectric Strength | 32.0 - 35.0 kV/mm | 813 - 889 kV/in | Average value: 33.7 kV/mm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |