Material Notes:
Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following important properties: High stiffnessHigh tensile strengthHigh heat distortion temperatureEmproved hydrolysis stability Application examples are stressed functional parts such as wheels, electrical bobbins, handles, levers and housings.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Water Absorption 5.0 %
5.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 130 MPa
18900 psi
conditioned; ISO 2039-1
230 MPa
33400 psi
dry; ISO 2039-1
Tensile Strength at Break 130 MPa
18900 psi
conditioned; ISO 527-1/-2
195 MPa
28300 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
6.0 %
6.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 7.00 GPa
1020 ksi
conditioned; ISO 527-1/-2
10.5 GPa
1520 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
dry; ISO 179/1eU
8.50 J/cm²
40.4 ft-lb/in²
conditioned; ISO 179/1eU
5.00 J/cm²

@Temperature 30.0 °C
23.8 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
5.50 J/cm²

@Temperature 30.0 °C
26.2 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
dry; ISO 179/1eA
1.50 J/cm²
7.14 ft-lb/in²
conditioned; ISO 179/1eA
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 130 - 150 °C
266 - 302 °F
long term; EMS
230 °C
446 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 190 °C
374 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 36.0 kV/mm
914 kV/in
conditioned; IEC 60243-1
39.0 kV/mm
991 kV/in
dry; IEC 60243-1
Comparative Tracking Index 550 V
550 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Powertrain and Chassis
Electricals & Electronics Electrical appliances
Form Granules
Industry & Consumer goods Heating systems
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Special Characteristics Improved heat resistance