Material Notes:
Aluminum cast plate ACP 6000 is a 7xxx series alloy surface-machined plate. This type of alloy ensures excellent machinability characteristics and adequate tensile strength. Thickness, flatness and surface finish offer very close tolerances.Information provided by ALIMEX GmbHHomogenized and stress relieved
Physical Properties Metric English Comments
Density 2.80 g/cc
0.101 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 65
65
Tensile Strength, Ultimate 165 MPa
23900 psi
Rm
Tensile Strength, Yield 105 MPa

@Strain 0.200 %
15200 psi

@Strain 0.200 %
Elongation at Break 3.0 %
3.0 %
Modulus of Elasticity 71.0 GPa
10300 ksi
Thermal Properties Metric English Comments
CTE, linear 24.3 µm/m-°C

@Temperature 20.0 °C
13.5 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 142 W/m-K
984 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000004778 ohm-cm
0.000004778 ohm-cm