ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Hot Rolled Plate, UNS N04400

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Hot Rolled Plate, UNS N04400.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequently applied in a range of environments ranging from mildly oxidizing through neutral and to moderately reducing conditions. An additional application area of the material is in marine environments and other nonoxidizing chloride solutions.. Specific uses include chemical or refining process equipment, pumps, valves, and fittings.The alloy has a long history of use as a corrosion resistant material, dating back to the early twentieth century when it was developed as an attempt to use a high copper content nickel ore. The nickel and copper contents of the ore were in the approximate ratio which is now formally specified for the alloy.As with commercially pure nickel, the AL 400 alloy is low in strength in the annealed condition. For this reason, a variety of tempers are used which have the effect of increasing the strength level of the material.Information provided by Allegheny Ludlum
Physical Properties Metric English Comments
Density 8.83 g/cc
0.319 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 70
70
Typical Annealed
Tensile Strength, Ultimate 550 MPa
79800 psi
Typical
Tensile Strength, Yield 310 MPa
45000 psi
Typical
Elongation at Break 30 %
30 %
Typical in 2"
Modulus of Elasticity 180 GPa
26100 ksi
Typical
Charpy Impact 135 - 325 J
99.6 - 240 ft-lb
Thermal Properties Metric English Comments
CTE, linear 13.9 µm/m-°C

@Temperature 20.0 - 93.0 °C
7.72 µin/in-°F

@Temperature 68.0 - 199 °F
15.8 µm/m-°C

@Temperature 20.0 - 315 °C
8.78 µin/in-°F

@Temperature 68.0 - 599 °F
16.4 µm/m-°C

@Temperature 20.0 - 538 °C
9.11 µin/in-°F

@Temperature 68.0 - 1000 °F
Specific Heat Capacity 0.430 J/g-°C
0.103 BTU/lb-°F
Thermal Conductivity 24.1 W/m-K
167 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 0.020 %
0.020 %
Carbon, C 0.10 %
0.10 %
Copper, Cu 32 %
32 %
Iron, Fe 1.0 %
1.0 %
Manganese, Mn 0.50 %
0.50 %
Nickel, Ni 66 %
66 %
as balance; includes Co
Phosphorous, P 0.0050 %
0.0050 %
Silicon, Si 0.25 %
0.25 %
Sulfur, S 0.0050 %
0.0050 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000510 ohm-cm
0.0000510 ohm-cm