Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh RigidityHigh StrengthLubricatedOil ResistantSolvent ResistantUses:BearingsBushingsCamsConnectors HousingsIndustrial ApplicationsAppearance: Natural ColorForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.4 %
2.4 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm

@Diameter 2.00 mm
0.022 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Diameter 2.00 mm
0.020 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527-2
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2
Elongation at Yield 20 %
20 %
ISO 527-2
Tensile Modulus 1.80 GPa
261 ksi
ISO 527-2
Flexural Strength 30.0 MPa
4350 psi
ISO 178
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180
20.0 kJ/m²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA