Material Notes:
AA-DUCT 916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good electrical and mechanical properties. AA-DUCT 916 is two-part, smooth paste adhesive of refined pure silver and epoxy resin components. It is free of solvents and copper or carbon additives. It develops strong, durable, resilient, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic insulates. AA-DUCT 916 cures at room temperature and can be used as a flexible "cold-solder" for heat-sensitive components where hot-soldering is impractical. It also can be used for the assembly and repair of electrical modules, flexible circuits, wave guides, flat cable and high frequency shields.Appearance: SilverCure Type: Heat cure or Room temperatureMix Ratio by weight: 100:115/Resin:Hardener Benefits: High strengthPerfect bondCold solder for heat sensitive components Substrates: Excellent choice aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards. Typical Application: It can be used as a flexible "cold-solder" for heat-sensitive components where hot-soldering is impractical. The assembly and repair of electrical modules, flexible circuits, wave guides, flat cable and high frequency shields.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 2.85 g/cc
2.85 g/cc
uncured
Solids Content 100 %
100 %
reactive, uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
cured
Thermal Properties Metric English Comments
Thermal Conductivity 1.50 W/m-K
10.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 5.00 °C
41.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.00010 ohm-cm
<= 0.00010 ohm-cm
cured
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 180 min
180 min
uncured
Shelf Life 12.0 Month
12.0 Month
uncured
Descriptive Properties Value Comments
Viscosity Paste
uncured
Users viewing this material also viewed the following: