Barlog Plastics KEBATER B511T PBT unreinforced, super tough

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade
Manufacturer Barlog Plastics
Trade Name KEBATER
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBATER B511T PBT unreinforced, super tough.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PBT-IInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.20 %
0.20 %
similar to ISO 62 test
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527-1
Elongation at Break 50 %
50 %
ISO 527-1
Tensile Modulus 1.80 GPa
261 ksi
ISO 527-1
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179-1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243-1
Descriptive Properties Value Comments
Resin Type PBT-I