Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 138 - 160 °C | 280 - 320 °F | Thermoforming Temp |
Alcoa KAMA 5100 CPET
(discontinued **) CapabilitiesGauge: .020" to .040" (508 to 106µm)Width: 20" to 52" (508 to 1321mm)Core size: 3" or 6"Roll O.D.: 29" standard, available up to 40"Silicone coating availableAvailable in natural blackP.. |
|||
Processing Temperature | 138 °C | 280 °F | curing temp. |
Arlon 0.008" (0.2032 mm) Thermabond®-45 Uncured Silicone (99720W008) 0.008 in., +0.000,-0.002(0.2 mm, +0.00, -0.05) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in +0.000,-0.002(0... |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | Molding |
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A30 General Purpose Molding Compound BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression mol.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the .. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applic.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T14 General Purpose Molding Compound BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cos.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T9 General Purpose Molding Compound BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T10(GP) General Purpose Molding Compound BMC T10(GP) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T10(GP) is well suited for injection, transfer or compression molding of intricate parts... |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T40(18)-LS Die Casting Replacement Grade Molding Compound BMC T40(18)-LS is a low shrink compound designed as a direct replacement for aluminum die casting applications. T40(18)-LS is UL recognized. Excellent mechanical properties and dimensional stabili.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T15(GPT) General Purpose Molding Compound BMC T15(GPT) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPT) is well suited for injection, transfer or compression.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific .. |