Chosun Refractories TCH-175S Torpedo Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories TCH-175S Torpedo Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.005886 GPa

@Temperature 110 °C,
Time 86400 sec
0.8537 ksi

@Temperature 230 °F,
Time 24.0 hour
0.007848 GPa

@Temperature 1350 °C,
Time 10800 sec
1.138 ksi

@Temperature 2460 °F,
Time 3.00 hour
0.00981 GPa

@Temperature 1500 °C,
Time 10800 sec
1.42 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 34.3 MPa

@Temperature 110 °C,
Time 86400 sec
4980 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
49.0 MPa

@Temperature 1350 °C,
Time 10800 sec
7110 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
58.8 MPa

@Temperature 1500 °C,
Time 10800 sec
8530 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1650 °C
3000 °F
limited
Shrinkage -0.0300 %

@Temperature 110 °C,
Time 86400 sec
-0.0300 %

@Temperature 230 °F,
Time 24.0 hour
0.10 %

@Temperature 1350 °C,
Time 10800 sec
0.10 %

@Temperature 2460 °F,
Time 3.00 hour
0.20 %

@Temperature 1500 °C,
Time 10800 sec
0.20 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 80 %
80 %
SiC 10 %
10 %
SiO2 5.0 %
5.0 %
Descriptive Properties Value Comments
Installation Method Casting, Vibrating
Material Required for Estimating(kg/?) 2,800
Water Required for Casting(%) 6.0
Users viewing this material also viewed the following: