Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Glass fiber Filled
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.5 MPa
5300 psi
ASTM D638
Flexural Yield Strength 37.9 MPa
5500 psi
ASTM D790
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm

@Temperature 22.8 °C
2.20 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 191 - 249 °C
375 - 480 °F
Mold Temperature 21.1 - 65.6 °C
70.0 - 150 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm