Clariant Renol PURSP0005 Polyurethane Elastomer, Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PURSP0005 Polyurethane Elastomer, Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.0 MPa
7100 psi
ASTM D792
Flexural Modulus 1.90 GPa
275 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm
2.80 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 188 - 210 °C
370 - 410 °F
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.000 - 0.345 MPa
0.000 - 50.0 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm