Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 1.81e+15 ohm-cm Grade Count:19 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 2.18e+15 ohm-cm Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 3.33e+16 ohm-cm Grade Count:6 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |
|||
Electrical Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 1000 - 3.00e+16 ohm-cm | 1000 - 3.00e+16 ohm-cm | Average value: 7.45e+15 ohm-cm Grade Count:11 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 1000 °C |
<= 1000 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek Alumina-Zirconia Composite, AZ-25 Information provided by CoorsTek. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 1000 °C |
<= 1000 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek Dura-Z™ MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 500 °C |
<= 1000 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 1000 °C |
<= 1000 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek Yttria Partially Stabilized Zirconia, YZTP, Sintered Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 1000 °C |
<= 1000 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek YZTP Yttria Partially Stabilized Zirconia, Hipped Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 1000 ohm-cm | 1000 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Algoflon® 35CAR PTFE; Petroleum Coke and Graphite
(discontinued **) Data provided by the manufacturer.35 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric p.. |
|||
Electrical Resistivity | 1000 ohm-cm | 1000 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Algoflon® 1.2CSC PTFE; Superconductive Carbon Filled
(discontinued **) Data provided by the manufacturer.1.2 wt.% Superconductive Carbon. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric prope.. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 6.43e+15 ohm-cm Grade Count:43 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 3.58e+15 ohm-cm Grade Count:28 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | <= 1000 ohm-cm | <= 1000 ohm-cm | IEC 60093 |
CENTROPLAST CENTROLEN PP LF Polypropylene conductive This material is a low density, easily machined plastic that can be welded and has good surface conductivity. Applications include filter heads and housings, conveyor equipment for flammable liquid.. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 5.41e+15 ohm-cm Grade Count:48 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |