DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperatures Excellent resistance to wear and low friction Outstanding flow for easy processing and exceptional design freedomStanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical propertiesKey Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
(DAM); ISO 1183
Water Absorption 8.0 %
8.0 %
DAM; Sim. to ISO 62
Moisture Absorption at Equilibrium 2.2 %
2.2 %
Humidity Absorption (DAM); Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
DAM; ISO 294-4
0.011 cm/cm
0.011 in/in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 140 MPa
20300 psi
ISO 527-1/-2
Elongation at Break 6.0 %
6.0 %
ISO 527-1/-2
Tensile Modulus 8.00 GPa
1160 ksi
ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²

@Temperature -30.0 °C
35.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
2.20 J/cm²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 5500 MPa
798000 psi
ISO 899-1
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
10°C/min (DAM); ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 4.7

@Frequency 1e+6 Hz
4.7

@Frequency 1e+6 Hz
IEC 60250
16

@Frequency 100 Hz
16

@Frequency 100 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm
508 kV/in
IEC 60243-1
Dissipation Factor 0.010

@Frequency 1e+6 Hz
0.010

@Frequency 1e+6 Hz
IEC 60250
0.060

@Frequency 100 Hz
0.060

@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 300 V
300 V
IEC 60112
Descriptive Properties Value Comments
Heat stabilized or stable to heat Yes
Injection molding Yes
Platable Yes
With Fillers Yes