Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® 1SVX-50H black 9288 PA1010-GF50

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® 1SVX-50H black 9288 PA1010-GF50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Grilamid 1SVX-50H black 9288 is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile. Key properties of Grilamid 1SBVX-50H LDS black: Raw materials based on renewable resources Excellent impact and notched impact strength Good stiffness and strength Improved warpage performance Improved flowability Easy processing High dimensional stability Good surface finish Good UV and chemical resistance Grilamid 1SVX-50H black 9288 is suitable for production of technical parts in the application fields of: Electrical and electronic devices Automotive Mechanical engineering Sports & leisure goodsInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Water Absorption 2.0 %
2.0 %
ISO 62
Moisture Absorption 0.600 %
0.600 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
conditioned; ISO 527-1/-2
200 MPa
29000 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
3.0 %
3.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 13.0 GPa
1890 ksi
conditioned; ISO 527-1/-2
14.5 GPa
2100 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 10.0 J/cm²
47.6 ft-lb/in²
dry; ISO 179/1eU
10.0 J/cm²
47.6 ft-lb/in²
conditioned; ISO 179/1eU
8.50 J/cm²

@Temperature 30.0 °C
40.4 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
8.50 J/cm²

@Temperature 30.0 °C
40.4 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
dry; ISO 179/1eA
2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
1.80 J/cm²

@Temperature 30.0 °C
8.57 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.80 J/cm²

@Temperature 30.0 °C
8.57 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
5.56 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 °C
212 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 160 °C
320 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Comparative Tracking Index 600 V
600 V
dry; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Compressed air systems
Exterior
Fuel systems
Hydraulic systems
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Lighting
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Bio based Polyamide
Improved flowability and demoulding
Special Characteristics High impact or impact modified
Improved UV resistance (outdoor use)
Light stabilized or stable to light
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved