EMS-Grivory Grivory® TR 90 PAMACM12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TR 90 PAMACM12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid TR 90 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 natural offers outstanding properties such as: Transparency and weathering stabilityUnlimited colorabilityStress crack resistanceToughness and stiffnessGood chemical resistanceHigh flexural fatigue strengthEU and FDA food approval Grilamid TR 90 natural is especially suited for injection moulded outdoor applications in the application fields of: OpticsAutomotiveMechanical engineeringSafety technologySanitaryDomestic appliancesElectro / ElectronicsInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Water Absorption 3.0 %
3.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 90.0 MPa
13100 psi
conditioned; ISO 2039-1
Tensile Strength, Yield 60.0 MPa
8700 psi
conditioned; ISO 527-1/-2
60.0 MPa
8700 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 6.0 %
6.0 %
conditioned; ISO 527-1/-2
6.0 %
6.0 %
dry; ISO 527-1/-2
Tensile Modulus 1.60 GPa
232 ksi
conditioned; ISO 527-1/-2
1.60 GPa
232 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
dry; ISO 179/1eA
1.30 J/cm²
6.19 ft-lb/in²
conditioned; ISO 179/1eA
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Maximum Service Temperature, Air 80.0 - 100 °C
176 - 212 °F
long term; EMS
120 °C
248 °F
short term; EMS
Transformation Temperature, Tg 155 °C
311 °F
10°C/min; ISO 11357-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 34.0 kV/mm
864 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Cooling and climate control
Fuel systems
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Lighting
Mobile phones and other portable devices
Food contact EU Requirements
FDA
Form Granules
Industry & Consumer goods Heating systems
Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Power transmission
Sanitary, water and gas supply
Sports & Leisure
Tools & Accessories
Medical FDA
USP VI
Optics Lenses
Optical components
Safety glasses
Spectacle frames
Sunglasses
Packaging Cosmetics / Personal care
Medical packaging
Non oriented film
Processing Injection Molding
Other Extrusion
Special Characteristics Transparent
Water Contact DVGW W270
KTW
NSF 61
WRAS