Eastman M2001-P Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman M2001-P Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
M2001-P polyethylene is suggested for applications such as spiral-wound can linings, release paper and photographic paper. M2001-P has been found to exhibit good barrier properties, temperature resistance, and stress crack resistance.Information supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D4883
Melt Flow 10.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 25.0 MPa
3630 psi
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Tensile Strength, Yield 27.0 MPa
3920 psi
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Elongation at Break 10 %
10 %
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Coating