Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Starglas FF006 HDPE, Glass Fiber Filled

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Glass fiber Filled
Manufacturer Eurostar Engineering Plastics
Trade Name Starglas
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starglas FF006 HDPE, Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 4.00 mm
0.0030 - 0.0050 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 5.80 GPa
841 ksi
ISO 527
Flexural Strength 77.0 MPa
11200 psi
ISO 178
Flexural Modulus 4.50 GPa
653 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80x10x4; ISO 180/1U
Processing Properties Metric English Comments
Zone 1 170 - 200 °C
338 - 392 °F
Zone 2 170 - 200 °C
338 - 392 °F
Zone 3 170 - 200 °C
338 - 392 °F
Melt Temperature 190 °C
374 °F
Mold Temperature 40.0 - 55.0 °C
104 - 131 °F
Drying Temperature 70.0 °C

@Time 7200 sec
158 °F

@Time 2.00 hour