Material Notes:
HexPly® 922-1 is a structural epoxy resin for general industrial applications and aerospace applications. HexPly® 922-1 has an exceptionally good hot/wet performance and a very high glass temperature with cure cycle versatility, low viscosity and high flow. HexPly® 922-1 can be processed using a wide range of techniques. The HexPly® 922-1 family is available in fabrics and UD tapes.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.265 g/cc
0.04570 lb/in³
Cured
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.0 MPa
8120 psi
ISO R527 type 1
Elongation at Yield 1.7 %
1.7 %
ISO R527 type 1
Tensile Modulus 4.05 GPa
587 ksi
ISO R527 type 1
Flexural Yield Strength 129 MPa
18700 psi
ISO 178
Flexural Modulus 3.44 GPa
499 ksi
ISO 178
Poissons Ratio 0.384
0.384
ISO R527 type 1
Fracture Toughness 0.490 MPa-m½
0.446 ksi-in½
Shear Modulus 1.46 GPa
212 ksi
Calculated
Toughness 51.0 J
37.6 ft-lb
Per square meter
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 190 - 220 °C
374 - 428 °F
DMTA