Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Honeywell Aegis™ H85MP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell Aegis™ H85MP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Aegis H85MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU Directive 2002/72/EC. It possesses the combination of strength, toughness and thermo-forming properties associated with nylon 6 as well as excellent heat, chemical, and abrasion resistance.Applications:Processed MeatFresh Red MeatPoultryFishCheeseDried FoodChilled Fruit JuicesInformation provided by Honeywell.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D1505
Water Absorption 0.70 %
0.70 %
Extractable Content
1.6 %
1.6 %
in 24 hours
Moisture Absorption at Equilibrium 2.7 %
2.7 %
at 50% RH
Water Absorption at Saturation 9.5 %
9.5 %
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atm
35.6 cc-mil/100 in²-24hr-atm
cc/m²/day, No thickness given
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atm
185 cc-mil/100 in²-24hr-atm
cc/m²/day, No thickness given
Viscosity Measurement 3.15
3.15
96% SAV
85
85
FAV; ASTM D789
Maximum Moisture Content 0.080
0.080
Melt Flow 3.5 g/10 min

@Load 1.00 kg,
Temperature 235 °C
3.5 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D3418
Processing Properties Metric English Comments
Middle Barrel Temperature 230 - 260 °C
446 - 500 °F
Cast Film
246 - 254 °C
475 - 489 °F
Tubular (Blown) Film
Adapter Temperature 260 °C
500 °F
Tubular (Blown) Film
260 - 266 °C
500 - 511 °F
Cast Film
Die Temperature 254 °C
490 °F
Tubular (Blown) Film
260 °C
500 °F
Cast Film
Melt Temperature 254 - 260 °C
489 - 500 °F
Tubular (Blown) Film
260 - 270 °C
500 - 518 °F
Cast Film
Moisture Content 0.040 %
0.040 %