Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 2010 M Polypropylene Mica Filled, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 4010 M Polypropylene Mica Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses:Pump PartsInformation provided by Multibase |
|||
Middle Barrel Temperature | 249 - 260 °C | 480 - 500 °F | |
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FRG7.5 Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FV699 PBT, 10% Glass Reinforced Structural Foam Grade, Low Shrinkage Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Middle Barrel Temperature | 238 - 260 °C | 460 - 500 °F | |
Ravago Manufacturing Americas Hybrid S464LG Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color: Natural, Chry.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H205QP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500. It possesses the combination.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well .. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E.. |
|||
Middle Barrel Temperature | 235 - 260 °C | 455 - 500 °F | Start Point: 245°C |
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 245°C |
Kingfa JH960 6610 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 235°C |
Kingfa PC-S609 Toughened PC Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Injection Molding |
LG Chemical LUMID GP1200A(W) PA6, Medium Viscosity Feature: Injection Molding, PA6, Medium ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000G PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 24968-12-5 and 103598-77-2Information provid.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | |
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Middle Barrel Temperature | 249 - 260 °C | 480 - 500 °F | |
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® SG5500 PBT+PET+GF50% Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5011 PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Middle Barrel Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis BC612WG Polypropylene Copolymer BC612WG is a polypropylene copolymer intended for injection molding. The product is available in natural but other colors can be provided on request. This material has excellent balanced mechanical.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Unitika AXF-1500-05 Dry Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Unitika UM-8400-20 Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 |
Eurostar Starflam PK0022E PA6, 10% Mineral Filled, Injection Molded PK0022E is a Halogen Free and Phosphorous Free, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3620Z22 or PA 10E6 U9 Z22)Information provided by Polymer Technology & Services, the Nor.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 |
Eurostar Starflam PW0042E PA6, 20% Mineral Filled, Injection Molded PW0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Reinforced, Polyamide 6 Injection MoldingInformation provided by Polymer Technology & Services, the North American exclus.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions. |