Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Middle Barrel Temperature = 260 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 204 - 260 °C
400 - 500 °F
Multibase Multi-Pro® 1505 R Polypropylene
Glass Fiber Reinforced, 15% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced
Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced
Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources TP-FR IM PBT, Impact Modified, Flame Retardant, Low Flow
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant
Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t..
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources TP-FV699 PBT, 10% Glass Reinforced Structural Foam Grade, Low Shrinkage
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced
Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced
Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Middle Barrel Temperature 249 - 260 °C
480 - 500 °F
PTS Tristar® PC-10FR-(18) 18 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 238 - 260 °C
460 - 500 °F
Ravago Manufacturing Americas Hybrid S464LG Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color: Natural, Chry..
Middle Barrel Temperature 230 - 260 °C
446 - 500 °F
Cast Film
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Middle Barrel Temperature 230 - 260 °C
446 - 500 °F
Injection Molding
LG Chemical LUMID GP1100A(W) PA6, Low Viscosity
Feature: Injection Molding, PA6, Low ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical
Middle Barrel Temperature 245 - 260 °C
473 - 500 °F
Injection Molding
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose
Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
Middle Barrel Temperature 240 - 260 °C
464 - 500 °F
Injection Molding
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility
Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG ..
Middle Barrel Temperature 250 - 260 °C
482 - 500 °F
Injection Molding
LG Chemical Lupox® SG5200 PBT+PET+GF20%
Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical
Middle Barrel Temperature 250 - 260 °C
482 - 500 °F
Injection Molding
LG Chemical Lupox® TE5100 PBT+PC+GF10%
Description: Injection Molding, PBT+PC+GF10%, High Impact resistant, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 30965-26-5, 103598-77-2 and 65997-17-3Information provided..
Middle Barrel Temperature 249 - 260 °C
480 - 500 °F
Mitsubishi Iupilon® H2000R 23 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 249 - 260 °C
480 - 500 °F
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 249 - 260 °C
480 - 500 °F
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled
793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc.
Middle Barrel Temperature 250 - 260 °C
482 - 500 °F
Lavergne VYPET VNT 1021 Polyester-PC Alloy
The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic..
Middle Barrel Temperature 240 - 260 °C
464 - 500 °F
Start Point: 255°C
Kingfa PA6-RG30 Flame Retardant, 30% Glass Fiber Reinforced PA6
Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech. Co., Ltd...
Middle Barrel Temperature 250 - 260 °C
482 - 500 °F
Injection Molding
LG Chemical Lupox® SG5500 PBT+PET+GF50%
Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
Middle Barrel Temperature 240 - 260 °C
464 - 500 °F
Unitika AX-1500 Dry
AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in..
Middle Barrel Temperature 240 - 260 °C
464 - 500 °F
Unitika AXF-1500-05 Conditioned
Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd.
Middle Barrel Temperature 240 - 260 °C
464 - 500 °F
Unitika AXG-1500-300 Conditioned
Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd.
Middle Barrel Temperature 240 - 260 °C
464 - 500 °F
Unitika U-8400H
U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than..
Middle Barrel Temperature 216 - 260 °C
420 - 500 °F
LTL Color Compounds ColorFast® JCT1000 Polycarbonate-ABS-SMA Alloy
Unique PC/ABS/SMA alloy with improved processing and reduced plate-outAll information provided by LTL Color Compounders, Inc.
Copyright © lookpolymers.com All Rights Reserved