Material Notes:
Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock test (MIL-I-46058C)Flammability (self extinguishing) (ASTM D635)Good resistance to solvents (IPC CC 830)Recommended Stripper: 1090 Cure Type: UV
Physical Properties Metric English Comments
Density 0.959 g/cc
0.0346 lb/in³
ASTM D1475
Solids Content 94 %
94 %
Fed Std 141 Method 4044
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Viscosity 300 cP
300 cP
Fed Std Method 4287
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00452 GPa
0.655 ksi
Thermal Properties Metric English Comments
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Glass Transition Temp, Tg >= 200 °C
>= 392 °F
Flash Point >= 37.8 °C
>= 100 °F
ASTM D56
Electrical Properties Metric English Comments
Surface Resistance 5.00e+10 ohm
5.00e+10 ohm
Moisture Resistance; MIL-I-46058C
Insulation Resistance 5.00e+14 ohm
5.00e+14 ohm
Insulation Resistance; MIL-I-46058C
Dielectric Constant 2.5
2.5
ASTM D1 50 65T
Dielectric Breakdown >= 1500 V
>= 1500 V
Dielectric Withstand; MIL-I-46058C
Dissipation Factor 0.010
0.010
ASTM D1 50 65T
Processing Properties Metric English Comments
Cure Time 0.167 - 0.333 min
0.00278 - 0.00556 hour
Value given for curing at 300 W/in; Optimum properties in 24 hrs.
Shelf Life 6.00 Month

@Temperature 23.0 °C
6.00 Month

@Temperature 73.4 °F
Descriptive Properties Value Comments
Coverage 750 ft²/gal