IRPC Polimaxx Polene 121PC Styrene Acrylonitrile

Category Polymer , Thermoplastic , SAN Polymer
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 121PC Styrene Acrylonitrile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN
Physical Properties Metric English Comments
Melt Flow 2.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93

@Thickness 6.35 mm,
Temperature 23.0 °C
93

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D648
Tensile Strength, Yield 70.6 MPa

@Temperature 23.0 °C
10200 psi

@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 118 MPa

@Temperature 23.0 °C
17100 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 3.73 GPa

@Temperature 23.0 °C
540 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 0.216 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.405 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.35 mm
178 °F

@Thickness 0.250 in
ASTM D648
Vicat Softening Point 108 °C

@Load 1.00 kg,
Thickness 3.17 mm
226 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 210 - 260 °C
410 - 500 °F
Drying Temperature 80.0 - 85.0 °C

@Time 7200 - 10800 sec
176 - 185 °F

@Time 2.00 - 3.00 hour