Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Imerys Bardenâ„¢ R Kaolin

Category Ceramic , Clay , Kaolin Clay , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name Barden™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys Bardenâ„¢ R Kaolin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Particle Size 0.30 µm
0.30 µm
median
0.50 µm
0.50 µm
72% finer than
1.0 µm
1.0 µm
86% finer than
2.0 µm
2.0 µm
93% finer than
5.0 µm
5.0 µm
97% finer than
10 µm
10 µm
99% finer than
20 µm
20 µm
99% finer than
pH 5.0
5.0
Component Elements Properties Metric English Comments
Al2O3 38.1 %
38.1 %
CaO 0.020 %
0.020 %
Fe2O3 1.6 %
1.6 %
K2O 0.20 %
0.20 %
Loss on Ignition(%) 13.5 %

@Temperature 950 °C
13.5 %

@Temperature 1740 °F
P2O5 0.10 %
0.10 %
SiO2 45.1 %
45.1 %
SO3 0.50 %
0.50 %
TiO2 1.5 %
1.5 %
Zinc, Zn 0.0027 %
0.0027 %
Descriptive Properties Value Comments
Color white
Users viewing this material also viewed the following: