Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
ASTM D1693
Melt Flow 0.25 - 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 - 0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
4.5 - 7.2 g/10 min

@Load 21.6 kg,
Temperature 190 °C
4.5 - 7.2 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
Mechanical Properties Metric English Comments
Flexural Modulus >= 1.00 GPa
>= 145 ksi
ASTM D790
Izod Impact, Notched >= 4.00 J/cm

@Temperature 23.0 °C
>= 7.49 ft-lb/in

@Temperature 73.4 °F
ASTM D256