Material Notes:
Description: Very high flowApplication: CompoundingInformation provided by NILIT.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.5 %
1.5 %
24h in H<sub>2</sub>O; sim. ISO 62
Water Absorption at Saturation 8.5 %
8.5 %
sim. ISO 62
Viscosity Measurement 36
36
relative viscosity (formic acid); ASTM D789
Linear Mold Shrinkage, Flow 0.013 cm/cm
0.013 in/in
Nilit
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ASTM D638
Tensile Modulus 3.00 GPa
435 ksi
ASTM D638
Flexural Strength 120 MPa
17400 psi
ASTM D790
Flexural Modulus 2.85 GPa
413 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Vicat Softening Point 240 °C
464 °F
49 N; ASTM D1525
255 °C
491 °F
9.8 N; ASTM D1525
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
>= 600 V
UL 746
Users viewing this material also viewed the following: